Thermal transport properties of CeNiSn — •Silke Paschen1, Bodo Wand1, Günter Sparn1, Frank Steglich1, and Toshiro Takabatake21MPI für Chemische Physik fester Stoffe, Nöthnitzer Str. 48, D - 01187 Dresden — 2Faculty of Science, Hiroshima University, Kagamiyama 1-3-1, Higashi-Hiroshima 739-8526, Japan

We present thermal conductivity κ and thermopower S measurements on high–quality single crystalline CeNiSn along the three crystallographic axes a, b, and c in the temperature range between 100 mK and 7 K and in magnetic fields of up to 8 T. Both κ and S are highly anisotropic. Sa(T) has a pronounced maximum of approximately 50 µV/K at 4.2 K. κb(T) is dominated by a maximum at 3.8 K. Smaller enhancements in the same temperature region are also observed for κa and κc. A magnetic field of 8 T applied along the a axis, which is the easy axis of magnetization, strongly suppresses all these enhancements. Between 2 K and 600 mK,κiT2, indicating dominant phonon–electron scattering. Below 300 mK, κi=kT with slopes k larger than estimated for the electronic thermal conductivity using the Wiedemann–Franz law. Thus, even at the lowest temperatures, κ appears to be phonon dominated. All this suggests that the above mentioned enhancements originate from the opening of an anisotropic pseudogap [1].

[1] M. Sera et al., Phys. Rev. B 55, 6421 (1997) and Refs. herein.

100% | Bildschirmansicht | English Version | Kontakt/Impressum/Datenschutz
DPG-Physik > DPG-Verhandlungen > 2000 > Regensburg