DS 34: Hard and Superhard Coatings
Donnerstag, 28. Februar 2008, 15:45–16:45, H 2032
|
15:45 |
DS 34.1 |
Doping of high quality c-BN films epitaxially grown on top of diamond(001) — •Hong Yin, Xuyang Wang, Ivan Pongrac, Paul Ziemann, Fabian Renaux, Michel Hecq, and Carla Bittencourt
|
|
|
|
16:00 |
DS 34.2 |
Abscheidung und Anwendungen von Kohlenstoffnitridschichten (CNX) für Bauteile und Werkzeuge — •Ulrike Springborn, Katharina Köster, Mohammad Djahanbakhsh, Rolf Wäsche, Martin Keunecke und Klaus Bewilogua
|
|
|
|
16:15 |
DS 34.3 |
Scanning probe microscopy based characterization of reactive sputter deposited coatings — •Thomas Klünsner, Gregor Hlawacek, Christian Teichert, Nazanin Fateh, Harald Köstenbauer, Gerardo Fontalvo, and Christian Mitterer
|
|
|
|
16:30 |
DS 34.4 |
AlCrVN - Design of high-temperature low-friction hard coatings — •Robert Franz, Jörg Neidhardt, Markus Lechthaler, Peter Polcik, and Christian Mitterer
|
|
|