10:30 |
O 88.1 |
Electron Stimulated Desorption of Vanadyl-Groups from Vanadium Oxide Thin Films on Ru(0001) probed with STM — •Piotr Igor Wemhoff, Ying Wang, and Niklas Nilius
|
|
|
|
10:30 |
O 88.2 |
Heterogeneous Adsorption and Local Ordering of Formic Acid on Magnetite (111) — •Marcus Creutzburg, Kai Sellschopp, Steffen Tober, Vedran Vonk, Heshmat Noei, Gregor B. Vonbun-Feldbauer, and Andreas Stierle
|
|
|
|
10:30 |
O 88.3 |
Atomic-Scale Studies of Hydroformylation on Rh1/Fe3O4(001) — •Manuel Ulreich, Zdeněk Jakub, Florian Kraushofer, Matthias Meier, Michael Schmid, Ulrike Diebold, Cesare Franchini, and Gareth S. Parkinson
|
|
|
|
10:30 |
O 88.4 |
Comparison of single Rh adatoms on α-Fe2O3(1102) and TiO2(110) stabilized by adsorbed water — •Lena Haager, Florian Kraushofer, Moritz Eder, Ali Rafsanjani-Abbasi, Giada Franceschi, Michele Riva, Panukorn Sombut, Marlene Atzmueller, Michael Schmid, Cesare Franchini, Ulrike Diebold, and Gareth S. Parkinson
|
|
|
|
10:30 |
O 88.5 |
Unravelling CO Adsorption on Model Single-Atom Catalysts (SAC) — Jan Hulva, •Matthias Meier, Roland Bliem, Zdenek Jakub, Florian Kraushofer, Michael Schmid, Ulrike Diebold, Cesare Franchini, and Gareth S. Parkinson
|
|
|
|
10:30 |
O 88.6 |
Rapid surface oxygen exchange at the hematite-water interface — Zdenek Jakub, Matthias Meier, Florian Kraushofer, Jan Balajka, Jiri Pavelec, Michael Schmid, Cesare Franchini, Ulrike Diebold, and •Gareth S. Parkinson
|
|
|
|
10:30 |
O 88.7 |
Real-time Dynamics During TiO2 Photocatalysis — •Michael Wagstaffe, Lukas Wenthaus, Adrian Dominguez-Castro, Thomas Frauenheim, Adriel Dominguez, Angel Rubio, Wilfried Wurth, Andreas Stierle, and Heshmat Noei
|
|
|
|
10:30 |
O 88.8 |
Interaction of formic acid with magnetite surfaces – the DFT perspective — •Kai Sellschopp, Marcus Creutzburg, Björn Arndt, Heshmat Noei, Andreas Stierle, Stefan Müller, and Gregor Vonbun-Feldbauer
|
|
|